 High density
                                                        High density
                                                     Low binder
                                                        Low binder
                                                     Semi-flexible mat
                                                        Semi-flexible mat
                                                     Customized lengths
                                                        Customized lengths
                                                     Fewer joints and
                                                             less wastage
                                                        Fewer joints and
                                                             less wastage
                                                    | Make / Brand | Rockinsul | 
| Material | Low resin bonded stone wool mattress | 
| Standard / Code | IS 8183, IS 3144, ASTM C592 | 
| Parameter | Values | Standards | 
|---|---|---|
| Thermal Conductivity (W/m.K) | 0.059 at 200oC mean temperature | IS 8183 | 
| Thermal Resistance (m2 K/W) | Calculated as per thickness and thermal conductivity of insulation | 
| Parameter | Values | Standards | 
|---|---|---|
| Non-combustibility | Non-combustible / Incombustible | BS 476 Part 4, IS 8183 | 
| Surface Burning Characteristics : Flame Spread Index | ≤ 25 | ASTM E84, UL 723 | 
| Surface Burning Characteristics : Smoke Developed Index | ≤ 50 | ASTM E84, UL 723 | 
| Water Vapour Sorption | Less than 5% by volume | ASTM C1104, ASTM C1104M | 
| Water Absorption (Kg/m2) | Less than 0.5 | BS 2972 Part 11 | 
| Shot content | < 25% | IS 3144, IS 8183 | 
| Sulphur / Chloride | Chloride : less than 20 ppm Sulphur content : less than 0.2% | IS 3144, IS 8183 | 
| Mold growth | No fungal growth | IS 3144, IS 8183 | 
| Alkalinity | 7 to 10 | IS 8183 | 
| Environment | Fire | Health Safety | 
|---|---|---|
|   |   |   |